| Alloy | Status (*) | Heat treatment | Tensile strength kg/mm² | Yield strength kg/mm² | Extension Percentage (%) |
Rockwell hardness B or C scale |
Conductive percentage %IACS |
C17200 |
A (TB00) |
42-60 | 14-28 | 35-60 | B45-85 | 15-19 | |
| AT (TF00) |
3 hr 330℃ | 116-140 | 91-123 | 3-10 | C36-42 | 22-28 | |
| C17510 / C17500 | A (TB00) |
24-39 | 14-28 | 20-35 | B20-50 | 20-35 | |
| AT (TF00) |
3 hr 480℃ |
70-84 |
56-70 |
10-25 |
B92-100 |
45-60 |